Hard chrome rod beside an HVOF carbide coated rod

HVOF vs Hard Chrome Plating: Which Lasts Longer?

Hard chrome plating has protected hydraulic rods, rolls and shafts for decades. But more and more plants are replacing it with HVOF (high-velocity oxygen fuel) carbide coatings. Here is how the two compare, and when each one makes sense.

How each coating is made

Hard chrome is electroplated: the part sits in a chromic acid bath and chromium builds up on its surface. HVOF is a thermal spray process: carbide or metal powder is fired at the part at very high speed, forming a dense, well-bonded coating.

Wear resistance

Tungsten carbide HVOF coatings are typically harder than hard chrome and hold up better against abrasion and erosion. In many applications they last several times longer before the part needs reworking.

Corrosion

Hard chrome naturally contains fine microcracks. Corrosive fluids can travel through them to the base metal, which is why chrome-plated rods often show pitting. A well-applied HVOF coating is dense, with very low porosity, so it gives a better barrier, especially when a corrosion-resistant matrix such as cobalt-chrome is chosen.

Fatigue and stress

Chrome plating can reduce the fatigue strength of a part. HVOF coatings usually have neutral or compressive stress, which is kinder to parts under cyclic load.

Health and regulation

Hard chrome plating uses hexavalent chromium, a known carcinogen. Regulations on its use are tightening around the world, and many OEMs now ask for chrome-free alternatives. HVOF uses no chromic acid bath.

Thickness and repair

HVOF can be applied thicker than chrome in one go, so it can also restore worn dimensions. Parts are ground or polished to size after spraying.

When hard chrome still makes sense

  • Very low-cost parts where life is not critical
  • Complex internal bores that a spray gun cannot reach
  • Applications where an existing approved specification calls for chrome

Bottom line

For rods, rolls, shafts and sleeves that wear out or pit in service, HVOF is usually the better long-term choice. See our HVOF coating service, or send us a photo of your part for advice.